Physical Properties |
Units |
SS 800 |
SS 1600 |
Test Method |
| Liner Density (Tex=g/100m) |
gm/km |
800±5% |
1600±5% |
ASTM D 578 |
| Tensile Strength at Break |
N |
>560 |
>1200 |
ASTM D 885 |
| Load @ 0.5% Elongation |
N |
>120 |
>250 |
ASTM D 885 |
| Load @ 1.0% Elongation |
N |
>210 |
>490 |
ASTM D 885 |
| Modulus of Elasticity |
N/mm2 |
>75000 |
>75000 |
ASTM D 885 |
| Elongation at Break |
% |
<3.5 |
<3.5 |
ASTM D 885 |
| Standard Width |
mm |
2.5±1.0 |
3.5± 1.0 |
ASTM D 885 |
| Strand Thickness |
mm |
0.2±0.1 |
0.35±0.1 |
ASTM D 885 |
| Package Weight |
mm |
11 |
12 |
ASTM D 885 |